General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.14 % Show Supplier Material materials with Absorción de agua of 0.14 % | dry | ISO 62 | at 23°C after 24h |
Bio-based content | 43 % Show Supplier Material materials with Bio-based content of 43 % | dry | ASTM D6866-12 Method B | |
Densidad | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.03 % Show Supplier Material materials with Moisture absorption of 0.03 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 45 [-] Show Supplier Material materials with Dureza Shore D of 45 [-] | dry | ISO 868 | 3s |
Elongación | 250 % Show Supplier Material materials with Elongación of 250 % | dry | ISO 527-1/-2 | |
700 % Show Supplier Material materials with Elongación of 700 % | dry | ISO 527-1/-2 | ||
Módulo de flexión | 0.1 GPa Show Supplier Material materials with Módulo de flexión of 0.1 GPa | dry | ISO 178 | |
Módulo elástico | 0.09 GPa Show Supplier Material materials with Módulo elástico of 0.09 GPa | dry | ISO 527-1/-2 | |
Resistencia a desgarros | 106 kN/m Show Supplier Material materials with Resistencia a desgarros of 106 kN/m | dry | ISO 34-1; Method B | |
107 kN/m Show Supplier Material materials with Resistencia a desgarros of 107 kN/m | dry | ISO 34-1; Method B | ||
Resistencia a la tracción | 17 MPa Show Supplier Material materials with Resistencia a la tracción of 17 MPa | dry | ISO 527-1/-2 | |
24 MPa Show Supplier Material materials with Resistencia a la tracción of 24 MPa | dry | ISO 527-1/-2 | Normal |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 180 °C Show Supplier Material materials with Temperatura de fusión of 180 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 38 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 38 °C | dry | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | Sim. to ISO 294-4 | Parallel | ||
1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | ISO 294-4 | Normal | ||
1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 230 °C | 39 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 39 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Smokable Sausage Casings, Phone case | |
Certifications | Food Contact, Yellow Card Available |