General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 5.3 % Show Supplier Material materials with Absorción de agua of 5.3 % | dry | Sim. to ISO 62 |
Densidad | 1.52 g/cm³ Show Supplier Material materials with Densidad of 1.52 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 1 % Show Supplier Material materials with Elongación of 1 % | dry | ISO 527-1/-2 | |
Módulo elástico | 7 GPa Show Supplier Material materials with Módulo elástico of 7 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 2.2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 2.2 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Conductividad térmica | 2.1 W/(m·K) Show Supplier Material materials with Conductividad térmica of 2.1 W/(m·K) | dry | ASTM E1461 | through plane | |
14.0 W/(m·K) Show Supplier Material materials with Conductividad térmica of 14.0 W/(m·K) | dry | ASTM E1461 | in plane | ||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | |
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | UL746B | 0.75 mm | |
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | dry | UL746B | 0.75 mm |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 1e+07 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+07 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 10000 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Heat Sinks in LED Lamps | |
Certifications | Yellow Card Available |