General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 3.2 % Show Supplier Material materials with Absorción de agua of 3.2 % | dry | ISO 62 | at 23°C after 24h |
11.5 % Show Supplier Material materials with Absorción de agua of 11.5 % | dry | Sim. to ISO 62 | ||
Densidad | 1.23 g/cm³ Show Supplier Material materials with Densidad of 1.23 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3.2 % Show Supplier Material materials with Moisture absorption of 3.2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-1/-2 | |
4 % Show Supplier Material materials with Elongación of 4 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | conditioned | ISO 178 | |
280 MPa Show Supplier Material materials with Flexural yield strength of 280 MPa | dry | ISO 178 | ||
Módulo de flexión | 5.8 GPa Show Supplier Material materials with Módulo de flexión of 5.8 GPa | conditioned | ISO 178 | |
11.5 GPa Show Supplier Material materials with Módulo de flexión of 11.5 GPa | dry | ISO 178 | ||
Módulo elástico | 13 GPa Show Supplier Material materials with Módulo elástico of 13 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | conditioned | ISO 527-1/-2 | |
200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 5.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5.5 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 15% Carbon Fiber |