General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.07 g/cm³ Show Supplier Material materials with Densidad of 1.07 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.2 % Show Supplier Material materials with Moisture absorption of 2.2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 35 % Show Supplier Material materials with Elongación of 35 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Elongación of 50 % | conditioned | ISO 527-1/-2 | ||
Elongation at yield | 4.4 % Show Supplier Material materials with Elongation at yield of 4.4 % | dry | ISO 527-1/-2 | |
21.6 % Show Supplier Material materials with Elongation at yield of 21.6 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 30 MPa Show Supplier Material materials with Flexural yield strength of 30 MPa | conditioned | ISO 178 | |
76 MPa Show Supplier Material materials with Flexural yield strength of 76 MPa | dry | ISO 178 | ||
Módulo de flexión | 0.65 GPa Show Supplier Material materials with Módulo de flexión of 0.65 GPa | conditioned | ISO 178 | |
2 GPa Show Supplier Material materials with Módulo de flexión of 2 GPa | dry | ISO 178 | ||
Módulo elástico | 0.63 GPa Show Supplier Material materials with Módulo elástico of 0.63 GPa | conditioned | ISO 527-1/-2 | |
2.1 GPa Show Supplier Material materials with Módulo elástico of 2.1 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 85 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 9e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 53 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 53 °C | dry | ISO 75-1/-2 | 2 MPa | |
87 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 87 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3 [-] Show Supplier Material materials with Constante dieléctrica of 3 [-] | dry | IEC 62631-2-1 | 1MHz |
4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 100 [-] Show Supplier Material materials with Factor de disipación of 100 [-] | dry | IEC 62631-2-1 | 100Hz |
180 [-] Show Supplier Material materials with Factor de disipación of 180 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 29.0 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 29.0 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 3e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 3e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 9e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 9e+12 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo de la masa derretida | 230 °C | 2 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 2 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 230 °C | 3 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 3 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|