General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.66 g/cm³ Show Supplier Material materials with Densidad of 1.66 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 1.7 % Show Supplier Material materials with Elongación of 1.7 % | dry | ISO 527-1/-2 | |
2.5 % Show Supplier Material materials with Elongación of 2.5 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 210 MPa Show Supplier Material materials with Flexural yield strength of 210 MPa | conditioned | ISO 178 | |
260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | dry | ISO 178 | ||
Módulo de flexión | 8.6 GPa Show Supplier Material materials with Módulo de flexión of 8.6 GPa | conditioned | ISO 178 | |
11.5 GPa Show Supplier Material materials with Módulo de flexión of 11.5 GPa | dry | ISO 178 | ||
Módulo elástico | 8.7 GPa Show Supplier Material materials with Módulo elástico of 8.7 GPa | conditioned | ISO 527-1/-2 | |
12.1 GPa Show Supplier Material materials with Módulo elástico of 12.1 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | conditioned | ISO 527-1/-2 | |
160 MPa Show Supplier Material materials with Resistencia a la tracción of 160 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | dry | ISO 179/1eA |
23 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 54 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 54 kJ/m² | dry | ISO 179/1eU |
23 °C | 64 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 64 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 213 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 213 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
5 [-] Show Supplier Material materials with Constante dieléctrica of 5 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 130 [-] Show Supplier Material materials with Factor de disipación of 130 [-] | dry | IEC 62631-2-1 | 100Hz |
190 [-] Show Supplier Material materials with Factor de disipación of 190 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 23 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 23 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 6e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 6e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 6e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 6e+12 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 225 V Show Supplier Material materials with Índice de seguimiento comparativo of 225 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | dry | ISO 294-4 | Parallel | |
0.9 % Show Supplier Material materials with Contracción of 0.9 % | dry | ISO 294-4 | Normal | ||
Velocidad de flujo de la masa derretida | 250 °C | 41 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 41 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 250 °C | 31 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 31 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |