General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.45 % Show Supplier Material materials with Absorción de agua of 0.45 % | dry | Sim. to ISO 62 |
Densidad | 1.67 g/cm³ Show Supplier Material materials with Densidad of 1.67 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 1.5 % Show Supplier Material materials with Elongación of 1.5 % | dry | ISO 527-1/-2 | |
Módulo elástico | 14 GPa Show Supplier Material materials with Módulo elástico of 14 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Conductividad térmica | 0.65 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.65 W/(m·K) | dry | ASTM E1461 | through plane | |
1.6 W/(m·K) Show Supplier Material materials with Conductividad térmica of 1.6 W/(m·K) | dry | ASTM E1461 | in plane | ||
Temperatura de flexión bajo carga | 235 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 235 °C | dry | ISO 75-1/-2 | 2 MPa | |
250 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 250 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 255 °C Show Supplier Material materials with Temperatura de fusión of 255 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 14.0 [-] Show Supplier Material materials with Constante dieléctrica of 14.0 [-] | dry | IEC 60250 | 1 |
Rigidez dieléctrica | 1.1 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 1.1 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 3e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 3e+11 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Foglamps, LED Headlight Lighting Modules and Lensholders, Lens holder Sun load, Bezel (Black) Sun load, LED module frame | |
Fillers | 35% Glass Fiber |