General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 2.2 % Show Supplier Material materials with Absorción de agua of 2.2 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.22 g/cm³ Show Supplier Material materials with Densidad of 1.22 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore A | 94 [-] Show Supplier Material materials with Dureza Shore A of 94 [-] | dry | ISO 868 | 3s | |
Dureza Shore D | 50 [-] Show Supplier Material materials with Dureza Shore D of 50 [-] | dry | ISO 868 | 3s | |
Elongación | 150 % Show Supplier Material materials with Elongación of 150 % | dry | ISO 527-1/-2 | ||
640 % Show Supplier Material materials with Elongación of 640 % | dry | ISO 527-1/-2 | |||
Módulo de flexión | 0.2 GPa Show Supplier Material materials with Módulo de flexión of 0.2 GPa | dry | ISO 178 | ||
120 °C | 0.07 GPa Show Supplier Material materials with Módulo de flexión of 0.07 GPa | dry | ISO 178 | ||
Módulo elástico | 0.17 GPa Show Supplier Material materials with Módulo elástico of 0.17 GPa | dry | ISO 527-1/-2 | ||
Resistencia a desgarros | 116 kN/m Show Supplier Material materials with Resistencia a desgarros of 116 kN/m | dry | ISO 34-1; Method B | ||
121 kN/m Show Supplier Material materials with Resistencia a desgarros of 121 kN/m | dry | ISO 34-1; Method B | |||
Resistencia a la tracción | 27 MPa Show Supplier Material materials with Resistencia a la tracción of 27 MPa | dry | ISO 527-1/-2 | ||
36 MPa Show Supplier Material materials with Resistencia a la tracción of 36 MPa | dry | ISO 527-1/-2 | Normal | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 63 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 63 °C | dry | ISO 75-1/-2 | 0.45 MPa | |
Temperatura de fusión | 202 °C Show Supplier Material materials with Temperatura de fusión of 202 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | -57.0 °C Show Supplier Material materials with Temperatura de transición del vidrio of -57.0 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.7 % Show Supplier Material materials with Contracción of 1.7 % | dry | ISO 294-4 | Parallel | |
1.8 % Show Supplier Material materials with Contracción of 1.8 % | dry | ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 230 °C | 2 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 2 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Clean Air Inlet Ducts, Cold Charged Air Ducts |