General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 3.1 % Show Supplier Material materials with Absorción de agua of 3.1 % | dry | ISO 62 | at 23°C after 24h |
11.3 % Show Supplier Material materials with Absorción de agua of 11.3 % | dry | Sim. to ISO 62 | ||
Densidad | 1.26 g/cm³ Show Supplier Material materials with Densidad of 1.26 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3 % Show Supplier Material materials with Moisture absorption of 3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 20 % Show Supplier Material materials with Elongación of 20 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |
Módulo de flexión | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | dry | ISO 178 | |
Módulo elástico | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 160 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 160 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Front End Accessory Drive Parts: Belt Tensioner,Damping bands, Shoes and Bushings | |
Fillers | Aramid Fiber |