General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 11 % Show Supplier Material materials with Absorción de agua of 11 % | dry | Sim. to ISO 62 |
Densidad | 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.12 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4.1 % Show Supplier Material materials with Elongation at yield of 4.1 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 84 MPa Show Supplier Material materials with Flexural yield strength of 84 MPa | dry | ISO 178 | |
Módulo de flexión | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | dry | ISO 178 | |
Módulo elástico | 2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 2.6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2.6 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 49 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 49 °C | dry | ISO 75-1/-2 | 2 MPa | |
76 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 76 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 193 °C Show Supplier Material materials with Temperatura de fusión of 193 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo de la masa derretida | 230 °C | 2.6 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 2.6 g/10min | dry | ISO 1133 |
Velocidad de flujo del volumen derretido | 230 °C | 2.3 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 2.3 cm³/10min | dry | ISO 1133 |
Viscosity number | 246 cm³/gr Show Supplier Material materials with Viscosity number of 246 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property |
---|