General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.11 g/cm³ Show Supplier Material materials with Densidad of 1.11 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 30 [-] Show Supplier Material materials with Dureza Shore D of 30 [-] | dry | ISO 868 | 3s |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.04 GPa Show Supplier Material materials with Módulo elástico of 0.04 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 19 MPa Show Supplier Material materials with Resistencia a la tracción of 19 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 195 °C Show Supplier Material materials with Temperatura de fusión of 195 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 34 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 34 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |