Akulon® F130-C3

Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® F130-C3

Los datos sobre este material han sido proporcionados por DSM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyValueConditionTesting Standard

Absorción de agua

9 %

Show Supplier Material materials with Absorción de agua of 9 %

dry

Sim. to ISO 62

Coefficient of friction, kinetic

1 [-]

Show Supplier Material materials with Coefficient of friction, kinetic of 1 [-]

dry

ISO 8295

Coefficient of friction, static

1.2 [-]

Show Supplier Material materials with Coefficient of friction, static of 1.2 [-]

dry

ISO 8295

Densidad

1.13 g/cm³

Show Supplier Material materials with Densidad of 1.13 g/cm³

dry

ISO 1183

Moisture absorption

2.8 %

Show Supplier Material materials with Moisture absorption of 2.8 %

dry

Sim. to ISO 62

Mecánica

PropertyValueConditionTesting StandardComment

Elongación

350 %

Show Supplier Material materials with Elongación of 350 %

dry

ISO 527-3

Parallel

Límite elástico

31 MPa

Show Supplier Material materials with Límite elástico of 31 MPa

dry

ISO 527-3

Parallel

Módulo elástico

0.46 GPa

Show Supplier Material materials with Módulo elástico of 0.46 GPa

dry

DSM-Method, 50 mm/min

Resistencia a la tracción

82 MPa

Show Supplier Material materials with Resistencia a la tracción of 82 MPa

dry

ISO 527-3

Parallel

Aplicaciones térmicas

PropertyValueConditionTesting StandardComment

Calor específico

1550 J/(kg·K)

Show Supplier Material materials with Calor específico of 1550 J/(kg·K)

dry

-

2250 J/(kg·K)

Show Supplier Material materials with Calor específico of 2250 J/(kg·K)

dry

Coeficiente de dilatación térmica

9e-07 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K

dry

ISO 11359-1/-2

Parallel

Temperatura de fusión

220 °C

Show Supplier Material materials with Temperatura de fusión of 220 °C

dry

ISO 11357-1/-3

10°C/min

Óptico

PropertyValueConditionTesting Standard

Transparencia

83

dry

DSM method

Rheological Properties

PropertyTemperatureValueConditionTesting Standard

Melt viscosity

260 °C

810 Pa·s

Show Supplier Material materials with Melt viscosity of 810 Pa·s

dry

DSM method, 260 °C

Viscosity number

196 cm³/gr

Show Supplier Material materials with Viscosity number of 196 cm³/gr

dry

ISO 307, 1157, 1628

Technological properties

Property
Certifications

Food Contact