General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 9.5 % Show Supplier Material materials with Absorción de agua of 9.5 % | dry | Sim. to ISO 62 |
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard |
---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 |
Módulo elástico | 3.2 GPa Show Supplier Material materials with Módulo elástico of 3.2 GPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 2 mm | |
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.1 [-] Show Supplier Material materials with Constante dieléctrica of 3.1 [-] | dry | IEC 62631-2-1 | 1MHz |
3.4 [-] Show Supplier Material materials with Constante dieléctrica of 3.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 65 [-] Show Supplier Material materials with Factor de disipación of 65 [-] | dry | IEC 62631-2-1 | 100Hz |
165 [-] Show Supplier Material materials with Factor de disipación of 165 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Viscosity number | 370 cm³/gr Show Supplier Material materials with Viscosity number of 370 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Stock Shapes for Various Industries | |
Certifications | Food Contact, Yellow Card Available |