General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.57 g/cm³ Show Supplier Material materials with Densidad of 1.57 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4.1 % Show Supplier Material materials with Elongación of 4.1 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 370 MPa Show Supplier Material materials with Flexural yield strength of 370 MPa | dry | ISO 178 | |
Módulo de flexión | 16 GPa Show Supplier Material materials with Módulo de flexión of 16 GPa | dry | ISO 178 | |
Módulo elástico | 15 GPa Show Supplier Material materials with Módulo elástico of 15 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 230 MPa Show Supplier Material materials with Resistencia a la tracción of 230 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 105 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 105 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 250 °C | 2 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 2 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |