General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 3.5 % Show Supplier Material materials with Absorción de agua of 3.5 % | dry | ISO 62 | at 23°C after 24h |
12.4 % Show Supplier Material materials with Absorción de agua of 12.4 % | dry | Sim. to ISO 62 | ||
Densidad | 1.17 g/cm³ Show Supplier Material materials with Densidad of 1.17 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3.4 % Show Supplier Material materials with Moisture absorption of 3.4 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 10 % Show Supplier Material materials with Elongación of 10 % | dry | ISO 527-1/-2 | |
15 % Show Supplier Material materials with Elongación of 15 % | conditioned | ISO 527-1/-2 | ||
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongation at yield of 20 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |
Módulo de flexión | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | dry | ISO 178 | |
Módulo elástico | 1 GPa Show Supplier Material materials with Módulo elástico of 1 GPa | conditioned | ISO 527-1/-2 | |
2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 105 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 105 kJ/m² | dry | ISO 179/1eU |
-30 °C | 120 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 120 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 150 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 150 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 8.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Difusividad térmica | 8.96e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 8.96e-08 mm²/s | dry | - | ||
Temperatura de flexión bajo carga | 190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Parallel |
2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 1000 g/cm³ Show Supplier Material materials with Density of melt of 1000 g/cm³ | dry | - | |
Specific heat capacity melt | 2780.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2780.0 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.253 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.253 W/(m·K) | dry | - | |
Viscosity number | 180 cm³/gr Show Supplier Material materials with Viscosity number of 180 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties