General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 1.3 % Show Supplier Material materials with Elongación of 1.3 % | dry | ISO 527-1/-2 | |
150 °C | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ISO 527-1/-2 | |
Módulo elástico | 26 GPa Show Supplier Material materials with Módulo elástico of 26 GPa | dry | ISO 527-1/-2 | |
150 °C | 11.8 GPa Show Supplier Material materials with Módulo elástico of 11.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 280 MPa Show Supplier Material materials with Resistencia a la tracción of 280 MPa | dry | ISO 527-1/-2 | |
150 °C | 117 MPa Show Supplier Material materials with Resistencia a la tracción of 117 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 330 °C Show Supplier Material materials with Temperatura de fusión of 330 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | 155 °C Show Supplier Material materials with Temperatura de transición del vidrio of 155 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Carbon Fiber |