General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.23 g/cm³ Show Supplier Material materials with Densidad of 1.23 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 55.0 [-] Show Supplier Material materials with Dureza Shore D of 55.0 [-] | dry | ISO 868 | 3s | |
Elongación | 150 % Show Supplier Material materials with Elongación of 150 % | dry | ISO 527-1/-2 | ||
610 % Show Supplier Material materials with Elongación of 610 % | dry | ISO 527-1/-2 | |||
Módulo de flexión | 0.31 GPa Show Supplier Material materials with Módulo de flexión of 0.31 GPa | dry | ISO 178 | ||
120 °C | 0.11 GPa Show Supplier Material materials with Módulo de flexión of 0.11 GPa | dry | ISO 178 | ||
Módulo elástico | 0.3 GPa Show Supplier Material materials with Módulo elástico of 0.3 GPa | dry | ISO 527-1/-2 | ||
Resistencia a desgarros | 131 kN/m Show Supplier Material materials with Resistencia a desgarros of 131 kN/m | dry | ISO 34-1; Method B | ||
137 kN/m Show Supplier Material materials with Resistencia a desgarros of 137 kN/m | dry | ISO 34-1; Method B | |||
Resistencia a la tracción | 30 MPa Show Supplier Material materials with Resistencia a la tracción of 30 MPa | dry | ISO 527-1/-2 | ||
41 MPa Show Supplier Material materials with Resistencia a la tracción of 41 MPa | dry | ISO 527-1/-2 | Normal | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 100 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 100 °C | dry | ISO 75-1/-2 | 0.45 MPa | |
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de reblandecimiento Vicat | 105 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 105 °C | dry | ISO 306 | 50°C/h 50N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 2.9 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 2.9 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Clean Air Inlet Ducts, Hot Charged Air Ducts, Cold Charged Air Ducts |