General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 5.9 % Show Supplier Material materials with Absorción de agua of 5.9 % | dry | Sim. to ISO 62 |
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-1/-2 |
3.5 % Show Supplier Material materials with Elongación of 3.5 % | dry | ISO 527-1/-2 | ||
7 % Show Supplier Material materials with Elongación of 7 % | conditioned | ISO 527-1/-2 | ||
120 °C | 10.4 % Show Supplier Material materials with Elongación of 10.4 % | dry | ISO 527-1/-2 | |
150 °C | 10.8 % Show Supplier Material materials with Elongación of 10.8 % | dry | ISO 527-1/-2 | |
160 °C | 11 % Show Supplier Material materials with Elongación of 11 % | dry | ISO 527-1/-2 | |
180 °C | 11.3 % Show Supplier Material materials with Elongación of 11.3 % | dry | ISO 527-1/-2 | |
200 °C | 11.6 % Show Supplier Material materials with Elongación of 11.6 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | conditioned | ISO 178 | |
305 MPa Show Supplier Material materials with Flexural yield strength of 305 MPa | dry | ISO 178 | ||
120 °C | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | |
160 °C | 95 MPa Show Supplier Material materials with Flexural yield strength of 95 MPa | dry | ISO 178 | |
Módulo de flexión | 6.5 GPa Show Supplier Material materials with Módulo de flexión of 6.5 GPa | conditioned | ISO 178 | |
10.7 GPa Show Supplier Material materials with Módulo de flexión of 10.7 GPa | dry | ISO 178 | ||
120 °C | 4.9 GPa Show Supplier Material materials with Módulo de flexión of 4.9 GPa | dry | ISO 178 | |
160 °C | 4.2 GPa Show Supplier Material materials with Módulo de flexión of 4.2 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 12 GPa Show Supplier Material materials with Módulo elástico of 12 GPa | dry | ISO 527-1/-2 |
7 GPa Show Supplier Material materials with Módulo elástico of 7 GPa | conditioned | ISO 527-1/-2 | ||
11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | dry | ISO 527-1/-2 | ||
100 °C | 5.1 GPa Show Supplier Material materials with Módulo elástico of 5.1 GPa | dry | ISO 527-1/-2 | |
120 °C | 4.8 GPa Show Supplier Material materials with Módulo elástico of 4.8 GPa | dry | ISO 527-1/-2 | |
150 °C | 4.3 GPa Show Supplier Material materials with Módulo elástico of 4.3 GPa | dry | ISO 527-1/-2 | |
160 °C | 4.0 GPa Show Supplier Material materials with Módulo elástico of 4.0 GPa | dry | ISO 527-1/-2 | |
200 °C | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 250 MPa Show Supplier Material materials with Resistencia a la tracción of 250 MPa | dry | ISO 527-1/-2 |
125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | conditioned | ISO 527-1/-2 | ||
195 MPa Show Supplier Material materials with Resistencia a la tracción of 195 MPa | dry | ISO 527-1/-2 | ||
100 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | |
120 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-1/-2 | |
150 °C | 82 MPa Show Supplier Material materials with Resistencia a la tracción of 82 MPa | dry | ISO 527-1/-2 | |
160 °C | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | dry | ISO 527-1/-2 | |
180 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 | |
200 °C | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | dry | ISO 179/1eA | |
23 °C | 24 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 24 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 1.1e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.1e-07 mm²/s | dry | - | |||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.71 mm | ||
Temperatura de flexión bajo carga | 210 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4.3 [-] Show Supplier Material materials with Constante dieléctrica of 4.3 [-] | dry | IEC 62631-2-1 | 1MHz |
4.8 [-] Show Supplier Material materials with Constante dieléctrica of 4.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 170 [-] Show Supplier Material materials with Factor de disipación of 170 [-] | dry | IEC 62631-2-1 | 100Hz |
220 [-] Show Supplier Material materials with Factor de disipación of 220 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | conditioned | IEC 60243-1 | |
35 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 35 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 500 V Show Supplier Material materials with Índice de seguimiento comparativo of 500 V | conditioned | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | dry | ISO 294-4 | Parallel | |
0.9 % Show Supplier Material materials with Contracción of 0.9 % | dry | ISO 294-4 | Normal | ||
Density of melt | 1150 g/cm³ Show Supplier Material materials with Density of melt of 1150 g/cm³ | dry | - | ||
Specific heat capacity melt | 2110 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2110 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.27 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K) | dry | - | ||
Velocidad de flujo de la masa derretida | 275 °C | 48 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 48 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 275 °C | 40 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 40 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Air inlet manifolds, Integrated Air Inlet Manifolds (up to 180°C), Charge Air Cooler Caps, Oil Sumps and Pans, Transmission Oil Pans, Rocker Valve Covers, Fans & Shrouds, Fuel System: Various Components | |
Certifications | Yellow Card Available | |
Fillers | 35% Glass Fiber |