General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 7.6 % Show Supplier Material materials with Absorción de agua of 7.6 % | dry | Sim. to ISO 62 |
Densidad | 1.24 g/cm³ Show Supplier Material materials with Densidad of 1.24 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.9 % Show Supplier Material materials with Elongación of 2.9 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 160 MPa Show Supplier Material materials with Flexural yield strength of 160 MPa | dry | ISO 178 | |
Módulo de flexión | 5 GPa Show Supplier Material materials with Módulo de flexión of 5 GPa | dry | ISO 178 | |
Módulo elástico | 5.8 GPa Show Supplier Material materials with Módulo elástico of 5.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 200 °C Show Supplier Material materials with Ball pressure temperature of 200 °C | dry | IEC 60695-10-2 | |||
Glow Wire Flammability Index | 675 °C Show Supplier Material materials with Glow Wire Flammability Index of 675 °C | dry | IEC 60695-2-12 | 0.8 mm | ||
675 °C Show Supplier Material materials with Glow Wire Flammability Index of 675 °C | dry | IEC 60695-2-12 | 3 mm | |||
Temperatura de flexión bajo carga | 190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 15% Glass Fiber |