General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 3.1 % Show Supplier Material materials with Absorción de agua of 3.1 % | dry | Sim. to ISO 62 |
Densidad | 1.66 g/cm³ Show Supplier Material materials with Densidad of 1.66 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 |
2.2 % Show Supplier Material materials with Elongación of 2.2 % | conditioned | ISO 527-1/-2 | ||
2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-1/-2 | ||
40 °C | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-1/-2 | |
80 °C | 2.1 % Show Supplier Material materials with Elongación of 2.1 % | dry | ISO 527-1/-2 | |
100 °C | 2.2 % Show Supplier Material materials with Elongación of 2.2 % | dry | ISO 527-1/-2 | |
120 °C | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-1/-2 | |
150 °C | 4.2 % Show Supplier Material materials with Elongación of 4.2 % | dry | ISO 527-1/-2 | |
160 °C | 4.3 % Show Supplier Material materials with Elongación of 4.3 % | dry | ISO 527-1/-2 | |
180 °C | 4.6 % Show Supplier Material materials with Elongación of 4.6 % | dry | ISO 527-1/-2 | |
200 °C | 4.4 % Show Supplier Material materials with Elongación of 4.4 % | dry | ISO 527-1/-2 | |
210 °C | 0.004 % Show Supplier Material materials with Elongación of 0.004 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 380 MPa Show Supplier Material materials with Flexural yield strength of 380 MPa | conditioned | ISO 178 | |
420 MPa Show Supplier Material materials with Flexural yield strength of 420 MPa | dry | ISO 178 | ||
80 °C | 220 MPa Show Supplier Material materials with Flexural yield strength of 220 MPa | conditioned | ISO 178 | |
80 °C | 350 MPa Show Supplier Material materials with Flexural yield strength of 350 MPa | dry | ISO 178 | |
120 °C | 280 MPa Show Supplier Material materials with Flexural yield strength of 280 MPa | dry | ISO 178 | |
160 °C | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
180 °C | 130 MPa Show Supplier Material materials with Flexural yield strength of 130 MPa | dry | ISO 178 | |
200 °C | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |
210 °C | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |
Módulo de flexión | 17.5 GPa Show Supplier Material materials with Módulo de flexión of 17.5 GPa | dry | ISO 178 | |
18 GPa Show Supplier Material materials with Módulo de flexión of 18 GPa | conditioned | ISO 178 | ||
80 °C | 15 GPa Show Supplier Material materials with Módulo de flexión of 15 GPa | conditioned | ISO 178 | |
80 °C | 17.3 GPa Show Supplier Material materials with Módulo de flexión of 17.3 GPa | dry | ISO 178 | |
120 °C | 16.7 GPa Show Supplier Material materials with Módulo de flexión of 16.7 GPa | dry | ISO 178 | |
160 °C | 8.3 GPa Show Supplier Material materials with Módulo de flexión of 8.3 GPa | dry | ISO 178 | |
180 °C | 7.1 GPa Show Supplier Material materials with Módulo de flexión of 7.1 GPa | dry | ISO 178 | |
200 °C | 6.6 GPa Show Supplier Material materials with Módulo de flexión of 6.6 GPa | dry | ISO 178 | |
210 °C | 6.4 GPa Show Supplier Material materials with Módulo de flexión of 6.4 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 19 GPa Show Supplier Material materials with Módulo elástico of 19 GPa | dry | ISO 527-1/-2 |
18 GPa Show Supplier Material materials with Módulo elástico of 18 GPa | dry | ISO 527-1/-2 | ||
18.5 GPa Show Supplier Material materials with Módulo elástico of 18.5 GPa | conditioned | ISO 527-1/-2 | ||
40 °C | 17.5 GPa Show Supplier Material materials with Módulo elástico of 17.5 GPa | dry | ISO 527-1/-2 | |
80 °C | 17.2 GPa Show Supplier Material materials with Módulo elástico of 17.2 GPa | dry | ISO 527-1/-2 | |
100 °C | 17 GPa Show Supplier Material materials with Módulo elástico of 17 GPa | dry | ISO 527-1/-2 | |
120 °C | 16 GPa Show Supplier Material materials with Módulo elástico of 16 GPa | dry | ISO 527-1/-2 | |
150 °C | 8.5 GPa Show Supplier Material materials with Módulo elástico of 8.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 7.6 GPa Show Supplier Material materials with Módulo elástico of 7.6 GPa | dry | ISO 527-1/-2 | |
180 °C | 6.8 GPa Show Supplier Material materials with Módulo elástico of 6.8 GPa | dry | ISO 527-1/-2 | |
200 °C | 6.3 GPa Show Supplier Material materials with Módulo elástico of 6.3 GPa | dry | ISO 527-1/-2 | |
210 °C | 6 GPa Show Supplier Material materials with Módulo elástico of 6 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 340 MPa Show Supplier Material materials with Resistencia a la tracción of 340 MPa | dry | ISO 527-1/-2 |
260 MPa Show Supplier Material materials with Resistencia a la tracción of 260 MPa | conditioned | ISO 527-1/-2 | ||
280 MPa Show Supplier Material materials with Resistencia a la tracción of 280 MPa | dry | ISO 527-1/-2 | ||
40 °C | 270 MPa Show Supplier Material materials with Resistencia a la tracción of 270 MPa | dry | ISO 527-1/-2 | |
80 °C | 230 MPa Show Supplier Material materials with Resistencia a la tracción of 230 MPa | dry | ISO 527-1/-2 | |
100 °C | 210 MPa Show Supplier Material materials with Resistencia a la tracción of 210 MPa | dry | ISO 527-1/-2 | |
120 °C | 180 MPa Show Supplier Material materials with Resistencia a la tracción of 180 MPa | dry | ISO 527-1/-2 | |
150 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | |
160 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | |
180 °C | 83 MPa Show Supplier Material materials with Resistencia a la tracción of 83 MPa | dry | ISO 527-1/-2 | |
200 °C | 71 MPa Show Supplier Material materials with Resistencia a la tracción of 71 MPa | dry | ISO 527-1/-2 | |
210 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 15.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13.5 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 14.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.5 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU | |
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | 0.75 mm | UL746B | ||
Temperatura de flexión bajo carga | 305 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 305 °C | dry | ISO 75-1/-2 | 2 MPa | ||
320 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 320 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 333 °C Show Supplier Material materials with Temperatura de fusión of 333 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | 150 °C Show Supplier Material materials with Temperatura de transición del vidrio of 150 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 43 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 43 kV/mm | dry | IEC 60243-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Faucet mixing valve, Pump Housings | |
Certifications | Food Contact, Drinking Water, Yellow Card Available | |
Fillers | 50% Glass Fiber |