General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 7.6 % Show Supplier Material materials with Absorción de agua of 7.6 % | dry | Sim. to ISO 62 |
Densidad | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 10 % Show Supplier Material materials with Elongación of 10 % | dry | ISO 527-1/-2 | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |
Módulo de flexión | 2.7 GPa Show Supplier Material materials with Módulo de flexión of 2.7 GPa | dry | ISO 178 | |
Módulo elástico | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 4.7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.7 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 80 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 80 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property |
---|