General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 71 % Show Supplier Material materials with Bio-based content of 71 % | dry | ASTM D6866-12 Method B |
Densidad | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3.5 % Show Supplier Material materials with Elongación of 3.5 % | dry | ISO 527-1/-2 | |
6.5 % Show Supplier Material materials with Elongación of 6.5 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 160 MPa Show Supplier Material materials with Flexural yield strength of 160 MPa | dry | ISO 178 | |
Módulo de flexión | 5 GPa Show Supplier Material materials with Módulo de flexión of 5 GPa | dry | ISO 178 | |
Módulo elástico | 3.8 GPa Show Supplier Material materials with Módulo elástico of 3.8 GPa | conditioned | ISO 527-1/-2 | |
5.6 GPa Show Supplier Material materials with Módulo elástico of 5.6 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 85 MPa Show Supplier Material materials with Resistencia a la tracción of 85 MPa | conditioned | ISO 527-1/-2 | |
125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 214 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 214 °C | dry | ISO 75-1/-2 | 2 MPa | |
242 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 242 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 250 °C Show Supplier Material materials with Temperatura de fusión of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact | |
Fillers | 15% Glass Fiber |