General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 1.8 % Show Supplier Material materials with Absorción de agua of 1.8 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.06 g/cm³ Show Supplier Material materials with Densidad of 1.06 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.12 % Show Supplier Material materials with Moisture absorption of 0.12 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 79 [-] Show Supplier Material materials with Dureza Shore A of 79 [-] | dry | ISO 868 | 15s |
80 [-] Show Supplier Material materials with Dureza Shore A of 80 [-] | dry | ISO 868 | 3s | |
Dureza Shore D | 18 [-] Show Supplier Material materials with Dureza Shore D of 18 [-] | dry | ISO 868 | 15s |
19 [-] Show Supplier Material materials with Dureza Shore D of 19 [-] | dry | ISO 868 | 3s | |
Elongación | 300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | |
980 % Show Supplier Material materials with Elongación of 980 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.02 GPa Show Supplier Material materials with Módulo elástico of 0.02 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 14.4 MPa Show Supplier Material materials with Resistencia a la tracción of 14.4 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 1 mm | UL746B | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 1 mm | UL746B | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 1 mm | UL746B | |
Temperatura de fusión | 165 °C Show Supplier Material materials with Temperatura de fusión of 165 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | -68 °C Show Supplier Material materials with Temperatura de transición del vidrio of -68 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.7 % Show Supplier Material materials with Contracción of 0.7 % | dry | Sim. to ISO 294-4 | Parallel | |
1 % Show Supplier Material materials with Contracción of 1 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 230 °C | 76 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 76 cm³/10min | dry | ISO 1133 | |
Viscosity number | 3.32 cm³/gr Show Supplier Material materials with Viscosity number of 3.32 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Smartwatch Straps | |
Certifications | Yellow Card Available |