General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 12.5 % Show Supplier Material materials with Absorción de agua of 12.5 % | dry | Sim. to ISO 62 |
Densidad | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | dry | ISO 1183 |
Moisture absorption | 3.2 % Show Supplier Material materials with Moisture absorption of 3.2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 6 % Show Supplier Material materials with Elongación of 6 % | dry | ISO 527-1/-2 | |
30 % Show Supplier Material materials with Elongación of 30 % | conditioned | ISO 527-1/-2 | ||
120 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
160 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
180 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
200 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 50 MPa Show Supplier Material materials with Flexural yield strength of 50 MPa | conditioned | ISO 178 | |
150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | ||
120 °C | 40 MPa Show Supplier Material materials with Flexural yield strength of 40 MPa | dry | ISO 178 | |
160 °C | 30 MPa Show Supplier Material materials with Flexural yield strength of 30 MPa | dry | ISO 178 | |
Límite elástico | 120 °C | 50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | dry | ISO 527-1/-2 |
160 °C | 40 MPa Show Supplier Material materials with Límite elástico of 40 MPa | dry | ISO 527-1/-2 | |
180 °C | 40 MPa Show Supplier Material materials with Límite elástico of 40 MPa | dry | ISO 527-1/-2 | |
200 °C | 35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | dry | ISO 527-1/-2 | |
Módulo de flexión | 1 GPa Show Supplier Material materials with Módulo de flexión of 1 GPa | conditioned | ISO 178 | |
3.2 GPa Show Supplier Material materials with Módulo de flexión of 3.2 GPa | dry | ISO 178 | ||
120 °C | 1.1 GPa Show Supplier Material materials with Módulo de flexión of 1.1 GPa | dry | ISO 178 | |
160 °C | 0.85 GPa Show Supplier Material materials with Módulo de flexión of 0.85 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 4 GPa Show Supplier Material materials with Módulo elástico of 4 GPa | dry | ISO 527-1/-2 |
1.2 GPa Show Supplier Material materials with Módulo elástico of 1.2 GPa | conditioned | ISO 527-1/-2 | ||
3.7 GPa Show Supplier Material materials with Módulo elástico of 3.7 GPa | dry | ISO 527-1/-2 | ||
120 °C | 1.1 GPa Show Supplier Material materials with Módulo elástico of 1.1 GPa | dry | ISO 527-1/-2 | |
140 °C | 1 GPa Show Supplier Material materials with Módulo elástico of 1 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.95 GPa Show Supplier Material materials with Módulo elástico of 0.95 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.9 GPa Show Supplier Material materials with Módulo elástico of 0.9 GPa | dry | ISO 527-1/-2 | |
200 °C | 0.8 GPa Show Supplier Material materials with Módulo elástico of 0.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | conditioned | ISO 527-1/-2 | |
100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 2.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2.5 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal |
8e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property |
---|