General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 9 % Show Supplier Material materials with Absorción de agua of 9 % | dry | Sim. to ISO 62 |
Densidad | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
120 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 117 MPa Show Supplier Material materials with Flexural yield strength of 117 MPa | dry | ISO 178 | |
120 °C | 17.2 MPa Show Supplier Material materials with Flexural yield strength of 17.2 MPa | dry | ISO 178 | |
Módulo de flexión | 3.0 GPa Show Supplier Material materials with Módulo de flexión of 3.0 GPa | dry | ISO 178 | |
120 °C | 0.43 GPa Show Supplier Material materials with Módulo de flexión of 0.43 GPa | dry | ISO 178 | |
Módulo elástico | 3 GPa Show Supplier Material materials with Módulo elástico of 3 GPa | dry | ISO 527-1/-2 | |
120 °C | 0.39 GPa Show Supplier Material materials with Módulo elástico of 0.39 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 120 °C | 39 MPa Show Supplier Material materials with Resistencia a la tracción of 39 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 9e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 3 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 3 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 3 mm | ||
Temperatura de flexión bajo carga | 70 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 70 °C | dry | ISO 75-1/-2 | 2 MPa | ||
215 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.3 [-] Show Supplier Material materials with Constante dieléctrica of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.6 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 90 [-] Show Supplier Material materials with Factor de disipación of 90 [-] | dry | IEC 62631-2-1 | 100Hz |
220 [-] Show Supplier Material materials with Factor de disipación of 220 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Viscosity number | 280 cm³/gr Show Supplier Material materials with Viscosity number of 280 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Timing drive systems |