General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 9.5 % Show Supplier Material materials with Absorción de agua of 9.5 % | dry | Sim. to ISO 62 |
Coefficient of friction, kinetic | 1 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 1 [-] | dry | ISO 8295 |
Coefficient of friction, static | 1.2 [-] Show Supplier Material materials with Coefficient of friction, static of 1.2 [-] | dry | ISO 8295 |
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
350 % Show Supplier Material materials with Elongación of 350 % | dry | ISO 527-3 | Parallel | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Límite elástico | 31 MPa Show Supplier Material materials with Límite elástico of 31 MPa | dry | ISO 527-3 | Parallel |
78 MPa Show Supplier Material materials with Límite elástico of 78 MPa | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.45 GPa Show Supplier Material materials with Módulo elástico of 0.45 GPa | dry | DSM-Method, 50 mm/min | |
2.7 GPa Show Supplier Material materials with Módulo elástico of 2.7 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 83 MPa Show Supplier Material materials with Resistencia a la tracción of 83 MPa | dry | ISO 527-3 | Parallel |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Calor específico | 1550 J/(kg·K) Show Supplier Material materials with Calor específico of 1550 J/(kg·K) | dry | - | |
2250 J/(kg·K) Show Supplier Material materials with Calor específico of 2250 J/(kg·K) | dry | |||
Coeficiente de dilatación térmica | 9e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel |
9e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Óptico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Transparencia | 83 | dry | DSM method |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt viscosity | 260 °C | 2250 Pa·s Show Supplier Material materials with Melt viscosity of 2250 Pa·s | dry | DSM method, 260 °C |
Viscosity number | 245 cm³/gr Show Supplier Material materials with Viscosity number of 245 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Food Packaging Films, Cheese Packaging Blown Film, Meat Packaging Blown Film, Fish Packaging Blown Film, Medical Packaging Blown Film | |
Certifications | Food Contact |