Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.36 g/cm³ Show Supplier Material materials with Densidad of 1.36 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | dry | ISO 527-1/-2 | |
7 % Show Supplier Material materials with Elongación of 7 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | conditioned | ISO 178 | |
210 MPa Show Supplier Material materials with Flexural yield strength of 210 MPa | dry | ISO 178 | ||
Módulo de flexión | 3.3 GPa Show Supplier Material materials with Módulo de flexión of 3.3 GPa | conditioned | ISO 178 | |
6.6 GPa Show Supplier Material materials with Módulo de flexión of 6.6 GPa | dry | ISO 178 | ||
Módulo elástico | 4.2 GPa Show Supplier Material materials with Módulo elástico of 4.2 GPa | conditioned | ISO 527-1/-2 | |
7.2 GPa Show Supplier Material materials with Módulo elástico of 7.2 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | conditioned | ISO 527-1/-2 | |
135 MPa Show Supplier Material materials with Resistencia a la tracción of 135 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA |
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 58.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 58.0 kJ/m² | dry | ISO 179/1eU |
23 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 165 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 165 °C | dry | ISO 75-1/-2 | 2 MPa | |
210 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.7 % Show Supplier Material materials with Contracción of 0.7 % | dry | Sim. to ISO 294-4 | Parallel | |
0.8 % Show Supplier Material materials with Contracción of 0.8 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 250 °C | 10 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 10 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |