General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 5.1 % Show Supplier Material materials with Absorción de agua of 5.1 % | dry | Sim. to ISO 62 |
Densidad | 1.43 g/cm³ Show Supplier Material materials with Densidad of 1.43 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Elongación | 1.9 % Show Supplier Material materials with Elongación of 1.9 % | conditioned | ISO 527-1/-2 | |||
2 % Show Supplier Material materials with Elongación of 2 % | dry | ISO 527-1/-2 | ||||
2.4 % Show Supplier Material materials with Elongación of 2.4 % | dry, conditioned | ISO 527-1/-2 | 1 mm | |||
120 °C | 3.5 % Show Supplier Material materials with Elongación of 3.5 % | dry | ISO 527-1/-2 | |||
160 °C | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | |||
200 °C | 5.5 % Show Supplier Material materials with Elongación of 5.5 % | dry | ISO 527-1/-2 | |||
Flexural yield strength | 260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | conditioned | ISO 178 | |||
290 MPa Show Supplier Material materials with Flexural yield strength of 290 MPa | dry | ISO 178 | ||||
80 °C | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | dry | ISO 178 | |||
120 °C | 180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | dry | ISO 178 | |||
160 °C | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | |||
200 °C | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |||
Módulo de flexión | 10.5 GPa Show Supplier Material materials with Módulo de flexión of 10.5 GPa | dry | ISO 178 | |||
11 GPa Show Supplier Material materials with Módulo de flexión of 11 GPa | conditioned | ISO 178 | ||||
80 °C | 10 GPa Show Supplier Material materials with Módulo de flexión of 10 GPa | dry | ISO 178 | |||
120 °C | 7.5 GPa Show Supplier Material materials with Módulo de flexión of 7.5 GPa | dry | ISO 178 | |||
160 °C | 4.5 GPa Show Supplier Material materials with Módulo de flexión of 4.5 GPa | dry | ISO 178 | |||
200 °C | 4 GPa Show Supplier Material materials with Módulo de flexión of 4 GPa | dry | ISO 178 | |||
Módulo elástico | 10.8 GPa Show Supplier Material materials with Módulo elástico of 10.8 GPa | dry | ISO 527-1/-2 | 1 mm | ||
11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | conditioned | ISO 527-1/-2 | ||||
11.3 GPa Show Supplier Material materials with Módulo elástico of 11.3 GPa | dry | ISO 527-1/-2 | ||||
11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | conditioned | ISO 527-1/-2 | ||||
120 °C | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | dry | ISO 527-1/-2 | |||
160 °C | 4.5 GPa Show Supplier Material materials with Módulo elástico of 4.5 GPa | dry | ISO 527-1/-2 | |||
200 °C | 4 GPa Show Supplier Material materials with Módulo elástico of 4 GPa | dry | ISO 527-1/-2 | |||
Resistencia a la tracción | 170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | conditioned | ISO 527-1/-2 | |||
190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | dry | ISO 527-1/-2 | ||||
190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | conditioned | ISO 527-1/-2 | at low thickness | |||
200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
120 °C | 125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | dry | ISO 527-1/-2 | |||
160 °C | 85 MPa Show Supplier Material materials with Resistencia a la tracción of 85 MPa | dry | ISO 527-1/-2 | |||
200 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | conditioned | ISO 179/1eA | ||
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | conditioned | ISO 179/1eU | ||
23 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3e-07 1/K | dry | ASTM D696 | Parallel | |
5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5e-07 1/K | dry | ASTM D696 | Normal | ||
Temperatura de flexión bajo carga | 305 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 305 °C | dry | ISO 75-1/-2 | 2 MPa | |
320 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 320 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 325 °C Show Supplier Material materials with Temperatura de fusión of 325 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 125 °C Show Supplier Material materials with Temperatura de transición del vidrio of 125 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.8 [-] Show Supplier Material materials with Constante dieléctrica of 3.8 [-] | dry | IEC 60250 | 10GHz |
3.9 [-] Show Supplier Material materials with Constante dieléctrica of 3.9 [-] | dry | IEC 60250 | 1GHz | |
3.9 [-] Show Supplier Material materials with Constante dieléctrica of 3.9 [-] | conditioned | IEC 60250 | 10GHz | |
4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | conditioned | IEC 60250 | 1GHz | |
4.5 [-] Show Supplier Material materials with Constante dieléctrica of 4.5 [-] | dry, conditioned | IEC 62631-2-1 | 1MHz | |
5 [-] Show Supplier Material materials with Constante dieléctrica of 5 [-] | dry, conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 120 [-] Show Supplier Material materials with Factor de disipación of 120 [-] | dry | IEC 60250 | 10GHz |
140 [-] Show Supplier Material materials with Factor de disipación of 140 [-] | dry | IEC 60250 | 1GHz | |
150 [-] Show Supplier Material materials with Factor de disipación of 150 [-] | dry, conditioned | IEC 62631-2-1 | 100Hz | |
150 [-] Show Supplier Material materials with Factor de disipación of 150 [-] | conditioned | IEC 60250 | 1GHz | |
150 [-] Show Supplier Material materials with Factor de disipación of 150 [-] | conditioned | IEC 60250 | 10GHz | |
280 [-] Show Supplier Material materials with Factor de disipación of 280 [-] | dry, conditioned | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 33 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 33 kV/mm | dry, conditioned | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry, conditioned | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | dry | ISO 294-4 | Parallel |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | ISO 294-4 | Normal | |
Spiral flow length | 110 | dry | - | 1.0 mm 1000 bar |
Viscosity number | 98 cm³/gr Show Supplier Material materials with Viscosity number of 98 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Audio Jack Connectors, Temperature Sensor, Speed Sensor, Positition Sensor | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |