General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.29 g/cm³ Show Supplier Material materials with Densidad of 1.29 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | dry | ISO 527-1/-2 | |
8 % Show Supplier Material materials with Elongación of 8 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 50 MPa Show Supplier Material materials with Flexural yield strength of 50 MPa | conditioned | ISO 178 | |
120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | ||
Módulo de flexión | 1.5 GPa Show Supplier Material materials with Módulo de flexión of 1.5 GPa | conditioned | ISO 178 | |
4 GPa Show Supplier Material materials with Módulo de flexión of 4 GPa | dry | ISO 178 | ||
Módulo elástico | 3.2 GPa Show Supplier Material materials with Módulo elástico of 3.2 GPa | conditioned | ISO 527-1/-2 | |
5.4 GPa Show Supplier Material materials with Módulo elástico of 5.4 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | conditioned | ISO 527-1/-2 | |
77 MPa Show Supplier Material materials with Resistencia a la tracción of 77 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2 kJ/m² | dry | ISO 179/1eA |
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | dry, conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo de la masa derretida | 230 °C | 80 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 80 g/10min | dry | ISO 1133 |
Velocidad de flujo del volumen derretido | 230 °C | 73 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 73 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Fiber |