General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.6 % Show Supplier Material materials with Absorción de agua of 0.6 % | dry | Sim. to ISO 62 |
Densidad | 0.83 g/cm³ Show Supplier Material materials with Densidad of 0.83 g/cm³ | dry | ISO 60 |
1.29 g/cm³ Show Supplier Material materials with Densidad of 1.29 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 70 [-] Show Supplier Material materials with Dureza Shore D of 70 [-] | dry | ISO 868 | 3s | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
250 % Show Supplier Material materials with Elongación of 250 % | dry | ISO 527-1/-2 | |||
Elongation at yield | 17 % Show Supplier Material materials with Elongation at yield of 17 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.8 GPa Show Supplier Material materials with Módulo elástico of 0.8 GPa | dry | ISO 527-1/-2 | ||
Resistencia a desgarros | 215 kN/m Show Supplier Material materials with Resistencia a desgarros of 215 kN/m | dry | ISO 34-1; Method B | ||
Resistencia a la tracción | 43 MPa Show Supplier Material materials with Resistencia a la tracción of 43 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.65e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.65e-06 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.65e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.65e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 5.54e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 5.54e-08 mm²/s | dry | - | |||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | UL746B | 2 mm | ||
Temperatura de flexión bajo carga | 120 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 120 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 221 °C Show Supplier Material materials with Temperatura de fusión of 221 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de reblandecimiento Vicat | 160 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 160 °C | dry | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.3 [-] Show Supplier Material materials with Constante dieléctrica of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.7 [-] Show Supplier Material materials with Constante dieléctrica of 3.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 300 [-] Show Supplier Material materials with Factor de disipación of 300 [-] | dry | IEC 62631-2-1 | 1MHz |
Rigidez dieléctrica | 23 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 23 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.75 % Show Supplier Material materials with Contracción of 1.75 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Normal | ||
Density of melt | 950 g/cm³ Show Supplier Material materials with Density of melt of 950 g/cm³ | dry | - | ||
Specific heat capacity melt | 1900 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1900 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.1 W/(m·K) | dry | - | ||
Velocidad de flujo del volumen derretido | 230 °C | 18 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 18 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Screw Drivers and Plyers, Optical Fiber loose buffer tubes, Optical Fiber Cable guides and connectors | |
Certifications | Yellow Card Available |