General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.43 g/cm³ Show Supplier Material materials with Densidad of 1.43 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.9 % Show Supplier Material materials with Moisture absorption of 0.9 % | dry | Sim. to ISO 62 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 248 °C Show Supplier Material materials with Temperatura de fusión of 248 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | 70 °C Show Supplier Material materials with Temperatura de transición del vidrio of 70 °C | dry | ISO 11357-1/-2 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Door panel, Wheel, Central Floor | |
Fillers | 60% Carbon Fiber |