General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.3 g/cm³ Show Supplier Material materials with Densidad of 1.3 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 3.6 % Show Supplier Material materials with Elongación of 3.6 % | dry | ISO 527-1/-2 |
3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-1/-2 | ||
5.3 % Show Supplier Material materials with Elongación of 5.3 % | conditioned | ISO 527-1/-2 | ||
120 °C | 8.5 % Show Supplier Material materials with Elongación of 8.5 % | dry | ISO 527-1/-2 | |
150 °C | 9.5 % Show Supplier Material materials with Elongación of 9.5 % | dry | ISO 527-1/-2 | |
Módulo elástico | -40 °C | 6.4 GPa Show Supplier Material materials with Módulo elástico of 6.4 GPa | dry | ISO 527-1/-2 |
4.5 GPa Show Supplier Material materials with Módulo elástico of 4.5 GPa | conditioned | ISO 527-1/-2 | ||
6.8 GPa Show Supplier Material materials with Módulo elástico of 6.8 GPa | dry | ISO 527-1/-2 | ||
120 °C | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-1/-2 | |
150 °C | 2.2 GPa Show Supplier Material materials with Módulo elástico of 2.2 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 140 MPa Show Supplier Material materials with Resistencia a la tracción of 140 MPa | dry | ISO 527-1/-2 |
70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | conditioned | ISO 527-1/-2 | ||
110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | ||
120 °C | 54 MPa Show Supplier Material materials with Resistencia a la tracción of 54 MPa | dry | ISO 527-1/-2 | |
150 °C | 46 MPa Show Supplier Material materials with Resistencia a la tracción of 46 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 42 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 42 kJ/m² | dry | ISO 179/1eA |
23 °C | 5.8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5.8 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 5.7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 5.7 kJ/m² | dry | ISO 179/1eU |
23 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 230 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 230 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Fillers | 15% Glass Fiber |