General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 6.6 % Show Supplier Material materials with Absorción de agua of 6.6 % | dry | Sim. to ISO 62 |
Densidad | 1.35 g/cm³ Show Supplier Material materials with Densidad of 1.35 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 10 % Show Supplier Material materials with Elongación of 10 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 115 MPa Show Supplier Material materials with Flexural yield strength of 115 MPa | dry | ISO 178 | |
Módulo de flexión | 4.6 GPa Show Supplier Material materials with Módulo de flexión of 4.6 GPa | dry | ISO 178 | |
Módulo elástico | 5.3 GPa Show Supplier Material materials with Módulo elástico of 5.3 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry | ISO 179/1eA |
23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | dry | ISO 179/1eU |
23 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 80 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 80 °C | dry | ISO 75-1/-2 | 2 MPa | |
180 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 180 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 30% Mineral Powder |