General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.7 % Show Supplier Material materials with Absorción de agua of 0.7 % | dry | ISO 62 | at 23°C after 24h |
6.2 % Show Supplier Material materials with Absorción de agua of 6.2 % | dry | Sim. to ISO 62 | ||
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.3 % Show Supplier Material materials with Moisture absorption of 2.3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 13 % Show Supplier Material materials with Elongación of 13 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongación of 20 % | conditioned | ISO 527-1/-2 | ||
100 °C | 19 % Show Supplier Material materials with Elongación of 19 % | dry | ISO 527-1/-2 | |
120 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
140 °C | 100 % Show Supplier Material materials with Elongación of 100 % | dry | ISO 527-1/-2 | |
160 °C | 100 % Show Supplier Material materials with Elongación of 100 % | dry | ISO 527-1/-2 | |
180 °C | 90 % Show Supplier Material materials with Elongación of 90 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | conditioned | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | ||
Flexural yield strength | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |
Límite elástico | 60 MPa Show Supplier Material materials with Límite elástico of 60 MPa | conditioned | ISO 527-1/-2 | |
75 MPa Show Supplier Material materials with Límite elástico of 75 MPa | dry | ISO 527-1/-2 | ||
100 °C | 43 MPa Show Supplier Material materials with Límite elástico of 43 MPa | dry | ISO 527-1/-2 | |
120 °C | 31 MPa Show Supplier Material materials with Límite elástico of 31 MPa | dry | ISO 527-1/-2 | |
160 °C | 21 MPa Show Supplier Material materials with Límite elástico of 21 MPa | dry | ISO 527-1/-2 | |
180 °C | 20 MPa Show Supplier Material materials with Límite elástico of 20 MPa | dry | ISO 527-1/-2 | |
Módulo de flexión | 2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | dry | ISO 178 | |
Módulo elástico | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-1/-2 | |
2.9 GPa Show Supplier Material materials with Módulo elástico of 2.9 GPa | conditioned | ISO 527-1/-2 | ||
100 °C | 1.7 GPa Show Supplier Material materials with Módulo elástico of 1.7 GPa | dry | ISO 527-1/-2 | |
120 °C | 0.8 GPa Show Supplier Material materials with Módulo elástico of 0.8 GPa | dry | ISO 527-1/-2 | |
140 °C | 0.5 GPa Show Supplier Material materials with Módulo elástico of 0.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.41 GPa Show Supplier Material materials with Módulo elástico of 0.41 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.4 GPa Show Supplier Material materials with Módulo elástico of 0.4 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | conditioned | ISO 527-1/-2 | |
75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | dry | ISO 527-1/-2 | ||
100 °C | 40 MPa Show Supplier Material materials with Resistencia a la tracción of 40 MPa | dry | ISO 527-1/-2 | |
120 °C | 30 MPa Show Supplier Material materials with Resistencia a la tracción of 30 MPa | dry | ISO 527-1/-2 | |
140 °C | 25 MPa Show Supplier Material materials with Resistencia a la tracción of 25 MPa | dry | ISO 527-1/-2 | |
160 °C | 20 MPa Show Supplier Material materials with Resistencia a la tracción of 20 MPa | dry | ISO 527-1/-2 | |
180 °C | 18 MPa Show Supplier Material materials with Resistencia a la tracción of 18 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry | ISO 179/1eA |
23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 135 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 135 kJ/m² | dry | ISO 179/1eU |
23 °C | 175 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 175 kJ/m² | dry | ISO 179/1eU | |
23 °C | 185 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 185 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
7.8e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.8e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 110 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 110 °C | dry | ISO 75-1/-2 | 2 MPa | |
200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 325 °C Show Supplier Material materials with Temperatura de fusión of 325 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 125 °C Show Supplier Material materials with Temperatura de transición del vidrio of 125 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 33 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 33 kV/mm | conditioned | IEC 60243-1 |
35 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 35 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry, conditioned | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | ISO 294-4 | Parallel |
1.9 % Show Supplier Material materials with Contracción of 1.9 % | dry | ISO 294-4 | Normal | |
Spiral flow length | 130 | dry | - | 1.0 mm 1000 bar |
165 | dry | - | 1.0 mm 1200 bar | |
Viscosity number | 98 cm³/gr Show Supplier Material materials with Viscosity number of 98 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property |
---|