General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.22 % Show Supplier Material materials with Absorción de agua of 0.22 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore A | 98 [-] Show Supplier Material materials with Dureza Shore A of 98 [-] | dry | ISO 868 | 3s | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.3 GPa Show Supplier Material materials with Módulo elástico of 0.3 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 32 MPa Show Supplier Material materials with Resistencia a la tracción of 32 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 5 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 208 °C Show Supplier Material materials with Temperatura de fusión of 208 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 90 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 90 °C | dry | ISO 306 | 50°C/h 50N |
Temperatura de transición del vidrio | -10 °C Show Supplier Material materials with Temperatura de transición del vidrio of -10 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 9 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 9 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|