General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 17 % Show Supplier Material materials with Elongación of 17 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Elongación of 50 % | conditioned | ISO 527-1/-2 | ||
Elongation at yield | 5.3 % Show Supplier Material materials with Elongation at yield of 5.3 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 40 MPa Show Supplier Material materials with Flexural yield strength of 40 MPa | conditioned | ISO 178 | |
119 MPa Show Supplier Material materials with Flexural yield strength of 119 MPa | dry | ISO 178 | ||
Módulo de flexión | 0.99 GPa Show Supplier Material materials with Módulo de flexión of 0.99 GPa | conditioned | ISO 178 | |
3 GPa Show Supplier Material materials with Módulo de flexión of 3 GPa | dry | ISO 178 | ||
Módulo elástico | 1 GPa Show Supplier Material materials with Módulo elástico of 1 GPa | conditioned | ISO 527-1/-2 | |
3.1 GPa Show Supplier Material materials with Módulo elástico of 3.1 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry | ISO 179/1eA |
23 °C | 31 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 31 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 57 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 57 °C | dry | ISO 75-1/-2 | 2 MPa | |
175 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 175 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
Factor de disipación | 220 [-] Show Supplier Material materials with Factor de disipación of 220 [-] | dry | IEC 62631-2-1 | 1MHz |
Rigidez dieléctrica | 26 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 26 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.2 % Show Supplier Material materials with Contracción of 1.2 % | dry | ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | ISO 294-4 | Normal | ||
Velocidad de flujo de la masa derretida | 230 °C | 34 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 34 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 230 °C | 30 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 30 cm³/10min | dry | ISO 1133 | |
Viscosity number | 138 cm³/gr Show Supplier Material materials with Viscosity number of 138 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property |
---|