Akulon® K122

Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® K122

Los datos sobre este material han sido proporcionados por DSM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyValueConditionTesting Standard

Absorción de agua

9.5 %

Show Supplier Material materials with Absorción de agua of 9.5 %

dry

Sim. to ISO 62

Densidad

1.13 g/cm³

Show Supplier Material materials with Densidad of 1.13 g/cm³

dry

ISO 1183

Moisture absorption

2.5 %

Show Supplier Material materials with Moisture absorption of 2.5 %

dry

Sim. to ISO 62

Mecánica

PropertyTemperatureValueConditionTesting Standard

Elongation at yield

4.2 %

Show Supplier Material materials with Elongation at yield of 4.2 %

dry

ISO 527-1/-2

Módulo elástico

2.7 GPa

Show Supplier Material materials with Módulo elástico of 2.7 GPa

dry

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

23 °C

5 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m²

dry

ISO 179/1eA

Aplicaciones térmicas

PropertyValueConditionTesting StandardComment

Difusividad térmica

8.82e-08 mm²/s

Show Supplier Material materials with Difusividad térmica of 8.82e-08 mm²/s

dry

-

Temperatura de fusión

220 °C

Show Supplier Material materials with Temperatura de fusión of 220 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyValueConditionTesting Standard

Density of melt

960 g/cm³

Show Supplier Material materials with Density of melt of 960 g/cm³

dry

-

Specific heat capacity melt

2680 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 2680 J/(kg·K)

dry

-

Thermal conductivity of melt

0.23 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.23 W/(m·K)

dry

-

Viscosity number

132 cm³/gr

Show Supplier Material materials with Viscosity number of 132 cm³/gr

dry

ISO 307, 1157, 1628

Technological properties

Property
Certifications

Food Contact