General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.6 % Show Supplier Material materials with Absorción de agua of 0.6 % | dry | ISO 62 | at 23°C after 24h |
4.8 % Show Supplier Material materials with Absorción de agua of 4.8 % | dry | Sim. to ISO 62 | ||
Bio-based content | 68 % Show Supplier Material materials with Bio-based content of 68 % | dry | ASTM D6866-12 Method B | |
Densidad | 1.16 g/cm³ Show Supplier Material materials with Densidad of 1.16 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 | |
Índice límite de óxigeno | 36 % Show Supplier Material materials with Índice límite de óxigeno of 36 % | dry | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Thickness |
---|---|---|---|---|---|
Elongación | 6 % Show Supplier Material materials with Elongación of 6 % | dry | ISO 527-1/-2 | ||
30 % Show Supplier Material materials with Elongación of 30 % | conditioned | ISO 527-1/-2 | |||
65 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
90 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
100 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
125 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | ||
12.5 % Show Supplier Material materials with Elongation at yield of 12.5 % | conditioned | ISO 527-1/-2 | |||
Flexural yield strength | 65 MPa Show Supplier Material materials with Flexural yield strength of 65 MPa | conditioned | ISO 178 | ||
120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | |||
Límite elástico | 50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | conditioned | ISO 527-1/-2 | ||
75 MPa Show Supplier Material materials with Límite elástico of 75 MPa | dry | ISO 527-1/-2 | |||
65 °C | 47 MPa Show Supplier Material materials with Límite elástico of 47 MPa | dry | ISO 527-1/-2 | ||
90 °C | 36 MPa Show Supplier Material materials with Límite elástico of 36 MPa | dry | ISO 527-1/-2 | ||
100 °C | 33 MPa Show Supplier Material materials with Límite elástico of 33 MPa | dry | ISO 527-1/-2 | ||
125 °C | 28.0 MPa Show Supplier Material materials with Límite elástico of 28.0 MPa | dry | ISO 527-1/-2 | ||
Módulo de flexión | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | conditioned | ISO 178 | ||
3.9 GPa Show Supplier Material materials with Módulo de flexión of 3.9 GPa | dry | ISO 178 | |||
Módulo elástico | 2.2 GPa Show Supplier Material materials with Módulo elástico of 2.2 GPa | conditioned | ISO 527-1/-2 | ||
3.4 GPa Show Supplier Material materials with Módulo elástico of 3.4 GPa | dry | ISO 527-1/-2 | 0.6 mm | ||
3.8 GPa Show Supplier Material materials with Módulo elástico of 3.8 GPa | dry | ISO 527-1/-2 | |||
65 °C | 1.9 GPa Show Supplier Material materials with Módulo elástico of 1.9 GPa | dry | ISO 527-1/-2 | ||
90 °C | 1.2 GPa Show Supplier Material materials with Módulo elástico of 1.2 GPa | dry | ISO 527-1/-2 | ||
100 °C | 1.1 GPa Show Supplier Material materials with Módulo elástico of 1.1 GPa | dry | ISO 527-1/-2 | ||
125 °C | 0.9 GPa Show Supplier Material materials with Módulo elástico of 0.9 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 2.8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2.8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | conditioned | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | dry | ISO 179/1eU | |
23 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 0.75 mm | IEC 60695-2-12 | ||
Glow Wire Ignition Temperature | 960 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 960 °C | dry | 0.75 mm | IEC 60695-2-13 | ||
Inflamabilidad | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.4 mm | UL746B | ||
Relative temperature index, mechanical impact | 95 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 95 °C | dry | 0.4 mm | UL746B | ||
Relative temperature index, mechanical strength | 115 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 115 °C | dry | 0.4 mm | UL746B | ||
Temperatura de flexión bajo carga | 110 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 110 °C | dry | ISO 75-1/-2 | 2 MPa | ||
190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 250 °C Show Supplier Material materials with Temperatura de fusión of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.45 [-] Show Supplier Material materials with Constante dieléctrica of 3.45 [-] | dry | IEC 62631-2-1 | 1MHz |
3.85 [-] Show Supplier Material materials with Constante dieléctrica of 3.85 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 140 [-] Show Supplier Material materials with Factor de disipación of 140 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Factor de disipación of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 27 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 27 kV/mm | conditioned | IEC 60243-1 | |
32 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 32 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 6e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 6e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 7e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 7e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry, conditioned | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |