General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.45 % Show Supplier Material materials with Absorción de agua of 0.45 % | dry | Sim. to ISO 62 |
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 10 % Show Supplier Material materials with Elongación of 10 % | dry | ISO 527-1/-2 |
13 % Show Supplier Material materials with Elongación of 13 % | dry | ISO 527-1/-2 | ||
120 °C | 130 % Show Supplier Material materials with Elongación of 130 % | dry | ISO 527-1/-2 | |
Elongation at yield | -40 °C | 7 % Show Supplier Material materials with Elongation at yield of 7 % | dry | ISO 527-1/-2 |
4.5 % Show Supplier Material materials with Elongation at yield of 4.5 % | dry | ISO 527-1/-2 | ||
Flexural yield strength | 75 MPa Show Supplier Material materials with Flexural yield strength of 75 MPa | dry | ISO 178 | |
120 °C | 17 MPa Show Supplier Material materials with Flexural yield strength of 17 MPa | dry | ISO 178 | |
160 °C | 8 MPa Show Supplier Material materials with Flexural yield strength of 8 MPa | dry | ISO 178 | |
Límite elástico | -40 °C | 90 MPa Show Supplier Material materials with Límite elástico of 90 MPa | dry | ISO 527-1/-2 |
50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | dry | ISO 527-1/-2 | ||
Módulo de flexión | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | dry | ISO 178 | |
120 °C | 0.38 GPa Show Supplier Material materials with Módulo de flexión of 0.38 GPa | dry | ISO 178 | |
160 °C | 0.16 GPa Show Supplier Material materials with Módulo de flexión of 0.16 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 3.4 GPa Show Supplier Material materials with Módulo elástico of 3.4 GPa | dry | ISO 527-1/-2 |
2.6 GPa Show Supplier Material materials with Módulo elástico of 2.6 GPa | dry | ISO 527-1/-2 | ||
100 °C | 0.45 GPa Show Supplier Material materials with Módulo elástico of 0.45 GPa | dry | ISO 527-1/-2 | |
120 °C | 0.35 GPa Show Supplier Material materials with Módulo elástico of 0.35 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.15 GPa Show Supplier Material materials with Módulo elástico of 0.15 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.15 GPa Show Supplier Material materials with Módulo elástico of 0.15 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | dry | ISO 527-1/-2 |
45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | dry | ISO 527-1/-2 | ||
100 °C | 25 MPa Show Supplier Material materials with Resistencia a la tracción of 25 MPa | dry | ISO 527-1/-2 | |
120 °C | 20 MPa Show Supplier Material materials with Resistencia a la tracción of 20 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA |
23 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 150 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 150 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 9e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
9e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 2 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |||
Glow Wire Ignition Temperature | 675 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 675 °C | dry | IEC 60695-2-13 | 2 mm | ||
900 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 900 °C | dry | IEC 60695-2-13 | 0.75 mm | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 60 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 60 °C | dry | ISO 75-1/-2 | 2 MPa | ||
140 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 140 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.2 [-] Show Supplier Material materials with Constante dieléctrica of 3.2 [-] | dry | IEC 62631-2-1 | 1MHz |
3.4 [-] Show Supplier Material materials with Constante dieléctrica of 3.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 30 [-] Show Supplier Material materials with Factor de disipación of 30 [-] | dry | IEC 62631-2-1 | 100Hz |
220 [-] Show Supplier Material materials with Factor de disipación of 220 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 2 % Show Supplier Material materials with Contracción of 2 % | dry | ISO 294-4 | Normal | |
2.3 % Show Supplier Material materials with Contracción of 2.3 % | dry | ISO 294-4 | Parallel | ||
Velocidad de flujo de la masa derretida | 250 °C | 4 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 4 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 250 °C | 5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 5 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | White Good Connectors | |