General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 12 % Show Supplier Material materials with Absorción de agua of 12 % | dry | Sim. to ISO 62 |
Densidad | 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.12 g/cm³ | dry | ISO 1183 |
Moisture absorption | 3.5 % Show Supplier Material materials with Moisture absorption of 3.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry, conditioned | ISO 527-1/-2 | |
Elongation at yield | 4.2 % Show Supplier Material materials with Elongation at yield of 4.2 % | dry | ISO 527-1/-2 | |
26 % Show Supplier Material materials with Elongation at yield of 26 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 32 MPa Show Supplier Material materials with Flexural yield strength of 32 MPa | conditioned | ISO 178 | |
108 MPa Show Supplier Material materials with Flexural yield strength of 108 MPa | dry | ISO 178 | ||
Módulo de flexión | 0.74 GPa Show Supplier Material materials with Módulo de flexión of 0.74 GPa | conditioned | ISO 178 | |
2.7 GPa Show Supplier Material materials with Módulo de flexión of 2.7 GPa | dry | ISO 178 | ||
Módulo elástico | 0.71 GPa Show Supplier Material materials with Módulo elástico of 0.71 GPa | conditioned | ISO 527-1/-2 | |
2.6 GPa Show Supplier Material materials with Módulo elástico of 2.6 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 47 MPa Show Supplier Material materials with Resistencia a la tracción of 47 MPa | dry | ISO 527-1/-2 | |
48 MPa Show Supplier Material materials with Resistencia a la tracción of 48 MPa | conditioned | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 2.4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2.4 kJ/m² | dry | ISO 179/1eA |
-30 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 5.3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5.3 kJ/m² | dry | ISO 179/1eA | |
23 °C | 51 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 51 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 54 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 54 °C | dry | ISO 75-1/-2 | 2 MPa | |
104 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 104 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Índice de seguimiento comparativo | - | dry | Sim. to IEC 60112 | Above 600V |
Technological properties
Property |
---|