General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 4.2 % Show Supplier Material materials with Absorción de agua of 4.2 % | dry | Sim. to ISO 62 |
Densidad | 1.63 g/cm³ Show Supplier Material materials with Densidad of 1.63 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Elongación | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | conditioned | ISO 527-1/-2 | |||
2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 | 1 mm | |||
2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | ISO 527-1/-2 | 1 mm | |||
Flexural yield strength | 350 MPa Show Supplier Material materials with Flexural yield strength of 350 MPa | conditioned | ISO 178 | |||
400 MPa Show Supplier Material materials with Flexural yield strength of 400 MPa | dry | ISO 178 | ||||
Módulo de flexión | 16.5 GPa Show Supplier Material materials with Módulo de flexión of 16.5 GPa | dry | ISO 178 | |||
17.5 GPa Show Supplier Material materials with Módulo de flexión of 17.5 GPa | conditioned | ISO 178 | ||||
Módulo elástico | 17.5 GPa Show Supplier Material materials with Módulo elástico of 17.5 GPa | dry | ISO 527-1/-2 | 1 mm | ||
17.5 GPa Show Supplier Material materials with Módulo elástico of 17.5 GPa | dry | ISO 527-1/-2 | 1 mm | |||
18.5 GPa Show Supplier Material materials with Módulo elástico of 18.5 GPa | conditioned | ISO 527-1/-2 | ||||
Resistencia a la tracción | 230 MPa Show Supplier Material materials with Resistencia a la tracción of 230 MPa | conditioned | ISO 527-1/-2 | |||
270 MPa Show Supplier Material materials with Resistencia a la tracción of 270 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
280 MPa Show Supplier Material materials with Resistencia a la tracción of 280 MPa | dry | ISO 527-1/-2 | 1 mm | |||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 12.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12.5 kJ/m² | conditioned | ISO 179/1eA | ||
23 °C | 14.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.5 kJ/m² | dry | ISO 179/1eA | |||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | conditioned | ISO 179/1eU | ||
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
4.8e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.8e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 245 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 245 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 315 °C Show Supplier Material materials with Temperatura de fusión of 315 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Antenna splitters, Camera Holder, Medium Voltage Circuit Breakers, Medium Voltage Circuit Breakers Embedded Pole, Free-form camera housing | |
Certifications | Yellow Card Available | |
Fillers | 50% Glass Fiber |