General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 4.2 % Show Supplier Material materials with Absorción de agua of 4.2 % | dry | Sim. to ISO 62 |
Densidad | 1.56 g/cm³ Show Supplier Material materials with Densidad of 1.56 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 | |
Módulo elástico | 16 GPa Show Supplier Material materials with Módulo elástico of 16 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 260 MPa Show Supplier Material materials with Resistencia a la tracción of 260 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 18 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 18 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Relative temperature index, electrical | 85 °C Show Supplier Material materials with Relative temperature index, electrical of 85 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 85 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 85 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 85 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 85 °C | dry | 0.75 mm | UL746B | ||
Temperatura de flexión bajo carga | 245 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 245 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Temperatura de fusión | 315 °C Show Supplier Material materials with Temperatura de fusión of 315 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |