General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.6 % Show Supplier Material materials with Absorción de agua of 0.6 % | dry | Sim. to ISO 62 |
Densidad | 1.28 g/cm³ Show Supplier Material materials with Densidad of 1.28 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.25 % Show Supplier Material materials with Moisture absorption of 0.25 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 55.0 [-] Show Supplier Material materials with Dureza Shore D of 55.0 [-] | dry | ISO 868 | 3s |
55.0 [-] Show Supplier Material materials with Dureza Shore D of 55.0 [-] | dry | ISO 868 | 15s | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
Elongation at yield | 22 % Show Supplier Material materials with Elongation at yield of 22 % | dry | ISO 527-1/-2 | |
Módulo elástico | 0.25 GPa Show Supplier Material materials with Módulo elástico of 0.25 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 27 MPa Show Supplier Material materials with Resistencia a la tracción of 27 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Inflamabilidad | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 2 mm | UL746B | ||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 2 mm | UL746B | ||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 2 mm | UL746B | ||
Temperatura de flexión bajo carga | 85 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 85 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 200 °C Show Supplier Material materials with Temperatura de fusión of 200 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de reblandecimiento Vicat | 90 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 90 °C | dry | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 5.2 [-] Show Supplier Material materials with Constante dieléctrica of 5.2 [-] | dry | IEC 62631-2-1 | 100Hz |
Factor de disipación | 0.02 [-] Show Supplier Material materials with Factor de disipación of 0.02 [-] | dry | IEC 62631-2-1 | 100Hz |
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.35 % Show Supplier Material materials with Contracción of 1.35 % | dry | Sim. to ISO 294-4 | Parallel | |
1.35 % Show Supplier Material materials with Contracción of 1.35 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo de la masa derretida | 230 °C | 14.4 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 14.4 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 230 °C | 15 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |