General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.23 g/cm³ Show Supplier Material materials with Densidad of 1.23 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.4 % Show Supplier Material materials with Moisture absorption of 2.4 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 | |
8.7 % Show Supplier Material materials with Elongación of 8.7 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | conditioned | ISO 178 | |
200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | dry | ISO 178 | ||
Módulo de flexión | 3 GPa Show Supplier Material materials with Módulo de flexión of 3 GPa | conditioned | ISO 178 | |
5.4 GPa Show Supplier Material materials with Módulo de flexión of 5.4 GPa | dry | ISO 178 | ||
Módulo elástico | 3.3 GPa Show Supplier Material materials with Módulo elástico of 3.3 GPa | conditioned | ISO 527-1/-2 | |
5.8 GPa Show Supplier Material materials with Módulo elástico of 5.8 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | conditioned | ISO 527-1/-2 | |
130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA |
23 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 39 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 39 kJ/m² | dry | ISO 179/1eU |
23 °C | 105 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 105 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 194 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 194 °C | dry | ISO 75-1/-2 | 2 MPa | |
216 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 216 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 100Hz |
4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz | |
Factor de disipación | 130 [-] Show Supplier Material materials with Factor de disipación of 130 [-] | dry | IEC 62631-2-1 | 100Hz |
230 [-] Show Supplier Material materials with Factor de disipación of 230 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 27 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 27 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 8e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 8e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 6e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 6e+12 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 400 V Show Supplier Material materials with Índice de seguimiento comparativo of 400 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | dry | ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | ISO 294-4 | Normal | ||
Velocidad de flujo de la masa derretida | 250 °C | 18 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 18 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 250 °C | 18 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 18 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 15% Glass Fiber |