General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.7 % Show Supplier Material materials with Absorción de agua of 0.7 % | dry | Sim. to ISO 62 |
Densidad | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 38 [-] Show Supplier Material materials with Dureza Shore D of 38 [-] | dry | ISO 868 | 3s |
Elongación | 210 % Show Supplier Material materials with Elongación of 210 % | dry | ISO 527-1/-2 | |
740 % Show Supplier Material materials with Elongación of 740 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.07 GPa Show Supplier Material materials with Módulo elástico of 0.07 GPa | dry | ISO 527-1/-2 | |
Resistencia a desgarros | 88 kN/m Show Supplier Material materials with Resistencia a desgarros of 88 kN/m | dry | ISO 34-1; Method B | |
103 kN/m Show Supplier Material materials with Resistencia a desgarros of 103 kN/m | dry | ISO 34-1; Method B | ||
Resistencia a la tracción | 17 MPa Show Supplier Material materials with Resistencia a la tracción of 17 MPa | dry | ISO 527-1/-2 | |
23 MPa Show Supplier Material materials with Resistencia a la tracción of 23 MPa | dry | ISO 527-1/-2 | Normal |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 203 °C Show Supplier Material materials with Temperatura de fusión of 203 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 230 °C | 10.5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 10.5 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Boots and Bellows |