Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 7 % Show Supplier Material materials with Elongación of 7 % | dry | ISO 527-1/-2 | |
Elongation at yield | 2.8 % Show Supplier Material materials with Elongation at yield of 2.8 % | dry | ISO 527-1/-2 | |
Módulo elástico | 3.5 GPa Show Supplier Material materials with Módulo elástico of 3.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 30 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Inflamabilidad | V-0 | dry | 1.6 mm | IEC 60695-11-10 | UL recognition :Yes |
Temperatura de fusión | 200 °C Show Supplier Material materials with Temperatura de fusión of 200 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 58.0 °C Show Supplier Material materials with Temperatura de transición del vidrio of 58.0 °C | dry | ISO 11357-1/-2 | 10°C/min |