General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1 % Show Supplier Material materials with Moisture absorption of 1 % | dry | Sim. to ISO 62 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | 80 °C Show Supplier Material materials with Temperatura de transición del vidrio of 80 °C | dry | ISO 11357-1/-2 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Fillers | 50 % Carbon Fiber |