General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 7.7 % Show Supplier Material materials with Absorción de agua of 7.7 % | dry | Sim. to ISO 62 |
Densidad | 1.21 g/cm³ Show Supplier Material materials with Densidad of 1.21 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.3 % Show Supplier Material materials with Moisture absorption of 2.3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | dry | ISO 527-1/-2 | |
9 % Show Supplier Material materials with Elongación of 9 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
Módulo de flexión | 4.2 GPa Show Supplier Material materials with Módulo de flexión of 4.2 GPa | dry | ISO 178 | |
Módulo elástico | 2.9 GPa Show Supplier Material materials with Módulo elástico of 2.9 GPa | conditioned | ISO 527-1/-2 | |
4.5 GPa Show Supplier Material materials with Módulo elástico of 4.5 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 68 MPa Show Supplier Material materials with Resistencia a la tracción of 68 MPa | conditioned | ISO 527-1/-2 | |
100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry | ISO 179/1eA |
-30 °C | 3.1 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3.1 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 3.8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3.8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.71 mm | ||
Temperatura de flexión bajo carga | 195 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 195 °C | dry | ISO 75-1/-2 | 2 MPa | ||
210 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 10% Glass Fiber |