General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 5.5 % Show Supplier Material materials with Absorción de agua of 5.5 % | Sim. to ISO 62 |
Densidad | 23.0 °C | 1.46 g/cm³ Show Supplier Material materials with Densidad of 1.46 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ISO 527-1/-2 |
Flexural yield strength | 23.0 °C | 285 MPa Show Supplier Material materials with Flexural yield strength of 285 MPa | ISO 178 |
Módulo de flexión | 23.0 °C | 11.4 GPa Show Supplier Material materials with Módulo de flexión of 11.4 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 13 GPa Show Supplier Material materials with Módulo elástico of 13 GPa | ISO 527-1/-2 |
Resistencia a la tracción | 23.0 °C | 210 MPa Show Supplier Material materials with Resistencia a la tracción of 210 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | ISO 179/1eA |
23.0 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 21 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30.0 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | ISO 179/1eU |
23.0 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | ISO 179/1eU | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2E-7 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2E-7 1/K | ISO 11359-1/-2, Parallel |
Coeficiente de dilatación térmica transversal | 23.0 °C | 5E-7 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 5E-7 1/K | ISO 11359-1/-2, Normal |
Heat deflection temperature, 0.45 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 220 °C | ISO 75-1/-2 | |
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75-1/-2 | |
Temperatura de flexión bajo carga | 205 - 220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 - 220 °C | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3, (10°C/min) |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 43% Glass Fiber |