General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 38 [-] Show Supplier Material materials with Dureza Shore D of 38 [-] | dry | ISO 868 | 3s |
Elongación | 275 % Show Supplier Material materials with Elongación of 275 % | dry | ISO 527-1/-2 | |
330 % Show Supplier Material materials with Elongación of 330 % | dry | ISO 527-1/-2 | ||
Módulo de flexión | 0.08 GPa Show Supplier Material materials with Módulo de flexión of 0.08 GPa | dry | ISO 178 | |
Módulo elástico | 0.09 GPa Show Supplier Material materials with Módulo elástico of 0.09 GPa | dry | ISO 527-1/-2 | |
Resistencia a desgarros | 97 kN/m Show Supplier Material materials with Resistencia a desgarros of 97 kN/m | dry | ISO 34-1; Method B | |
105 kN/m Show Supplier Material materials with Resistencia a desgarros of 105 kN/m | dry | ISO 34-1; Method B | ||
Resistencia a la tracción | 13 MPa Show Supplier Material materials with Resistencia a la tracción of 13 MPa | dry | ISO 527-1/-2 | Normal |
14.0 MPa Show Supplier Material materials with Resistencia a la tracción of 14.0 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.6 % Show Supplier Material materials with Contracción of 1.6 % | dry | Sim. to ISO 294-4 | Parallel | |
1.75 % Show Supplier Material materials with Contracción of 1.75 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 230 °C | 23 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 23 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Body Plugs |