General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 44 [-] Show Supplier Material materials with Dureza Shore D of 44 [-] | dry | ISO 868 | 3s |
Elongación | 165 % Show Supplier Material materials with Elongación of 165 % | dry | ISO 527-1/-2 | |
320 % Show Supplier Material materials with Elongación of 320 % | dry | ISO 527-1/-2 | ||
Módulo de flexión | 0.16 GPa Show Supplier Material materials with Módulo de flexión of 0.16 GPa | dry | ISO 178 | |
Módulo elástico | 0.17 GPa Show Supplier Material materials with Módulo elástico of 0.17 GPa | dry | ISO 527-1/-2 | |
Resistencia a desgarros | 74 kN/m Show Supplier Material materials with Resistencia a desgarros of 74 kN/m | dry | ISO 34-1; Method B | |
75 kN/m Show Supplier Material materials with Resistencia a desgarros of 75 kN/m | dry | ISO 34-1; Method B | ||
Resistencia a la tracción | 15 MPa Show Supplier Material materials with Resistencia a la tracción of 15 MPa | dry | ISO 527-1/-2 | |
16 MPa Show Supplier Material materials with Resistencia a la tracción of 16 MPa | dry | ISO 527-1/-2 | Normal |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 217 °C Show Supplier Material materials with Temperatura de fusión of 217 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.6 % Show Supplier Material materials with Contracción of 1.6 % | dry | Sim. to ISO 294-4 | Parallel | |
1.6 % Show Supplier Material materials with Contracción of 1.6 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 230 °C | 12.5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 12.5 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|